| Family: | Other |
| Weight: | 143.940 |
| Expansion: | 0.094 |
| Fusion: | 795C |
Molybdic Disulfide, Trioxide
-In glazes, glasses, and bodies, small amounts (-0.2%) act as a wetting agent during the melt phase. It lowers surface tension dramatically. This can encourage the development of crystals in crystalline glazes. Moly can give an iridescent quality to crystals and lustres.
-Also used in enamels as an adherence promoter and in some stains.
-It oxidizes quickly above 800F.
PropertiesFusion - 801CFrom The Oxide Handbook
AuthorsOthers: Ag2O, As2O3, As4O6, Au2O3, BeO, Bi2O3, CdO, CeO2, Cl, Cs2O, CuCO3, Dy2O3, Er2O3, Eu2O3, F, Fr2O, Free SiO2, Ga2O3, GdO3, GeO2, HfO2, HgO, Ho2O3, In2O3, IrO2, KNaO, La2O3, Lu2O3, Mn2O3, MoO3, N2O5, Nb2O5, Nd2O3, Ni2O3, OsO2, Pa2O5, PdO, PmO3, PO4, Pr2O3, PrO2, PtO2, RaO, Rb2O, Re2O7, RhO3, RuO2, Sb2O3, Sb2O5, Sc2O3, Se, Sm2O3, Ta2O5, Tb2O3, Tc2O7, ThO2, Tl2O, Tm2O3, Trace, U3O8, UO2, WO3, Y2O3, Yb2O3, |
Much more information with complete interlinking to many related databases can be found by logging into the www.ceramicmaterials.info database
Copyright 2003 http://digitalfire.com, All Rights Reserved
Please support http://ceramicmaterials.info to improve this library
|  |
INSIGHT is ceramic chemistry
calculation software that runs on
Windows, Mac and Linux and talks
to this web site. |
|